Overview of the different grades:
Spring wire grades
Chemical Composition of Cold Drawn Spring Steel Wire of Different Grades The chemical composition according to the heat analysis shall comply with the limit values shown in Table below or similar. The permissible deviation of the product analysis from the heat analysis is in accordance with EN 10016-2 and EN 10016-4 or similar.
Chemical composition, % by mass
NOTE
Some diameter ranges require particular attention for residuals. Therefore no figures are mentioned for chromium, nickel, molybdenum,tin, etc. leaving room for special arrangements between purchaser and supplier, dependent on their mutual processing conditions. This is also the case for the aluminium content.